EP3259239 (A2)

An environmentally sustainable cement composition, its use for inerting dredging sediments/sludges, relative method and apparatus for inerting

(22) 16.02.2016

(43) 27.12.2017

(57) Summary of the corresponding patent WO2016132286 (A2): A cement composition based on a sulfoaluminate clinker is described, together with its use for agglomerating and inerting sediment /dredging sludge, and the relative inerting method and apparatus.

(71) Italcementi S.p.A.; Ticass S.c.r.l. Tecnologie Innovative per Il Controllo Ambientale e lo Sviluppo Sostenibile; Università degli Studi di Genova (IT)

x

Related articles:

Issue 1/2021 RU 2 736 592 C1

Method of producing and composition of belite clinker

(22) 21.02.2020 (45) 18.11.2020 (57) Field: chemistry. Substance: disclosed group of inventions relates to a method of producing belite clinker and a composition of belite clinker. Method involves...

more
Issue 7/2021 EP 3 865 801 A1

Apparatus and method for manufacturing cement clinker

(22) 18.02.2020 (43) 18.08.2021 (57) A calciner 18 for receiving raw meal 102 from a preheater 20 of a cement clinker line 1, for calcining the raw meal 102 and for providing the calcined and/or...

more
Issue 4/2019 US 2019/0041342 A1

Analysis apparatus, analysis method and analysis program

(22) 15.02.2017 (43) 07.02.2019 (57) An analysis apparatus, an analysis method, and an analysis program by which even unskilled ones can perform quantitative analysis of a composition of...

more
Issue 3/2017 WO 2016/206785 A1

Mineralizer for calcium sulfoaluminate ternesite cements

(22) 16.06.2016 (43) 29.12.2016 (57) The present invention relates to a method for the production calcium sulfoaluminate (belite, ferrite) ternesite clinker using fluxes/mineralizers comprising the...

more
Issue 7-8/2020 WO 2020/052269 A1

Cement clinker preparation method and apparatus

(22) 21.05.2019 (43) 19.03.2020 (57) A cement clinker preparation method, comprising applying a voltage to a blank to fire the blank to obtain cement clinker under the condition of 900-1200 °C,...

more