ARTICLE

Effect of cement content on the performance of static cracking agent

Conventional blasting for rock and concrete demolition in sensitive environments inevitably generates adverse effects such as excessive noise, vibration, and flying rocks. To avoid these problems, static cracking agents (SCAs) provide a safer and more practical alternative by fracturing rock or concrete through the substantial volumetric expansion associated with the hydration of CaO to Ca(OH)2. However, conventional SCA suffers from inherent drawbacks, including relatively rapid hydration reaction rates and unstable expansion performance. To address these limitations, this study focuses on regulating the hydration reaction process and expansion performance of SCA by adjusting the proportion of cementitious materials in their composition. The experimental results show that a cement content of 12% provides the optimal expansion performance, with a volumetric expansion ratio of approximately 600%. Meanwhile, the hydration reaction is effectively moderated, and the peak temperature occurs at approximately 15 min. The mixture containing 10% cement exhibited the earliest crack initiation and the highest average crack-width development rate of 4.50 mm/min, whereas the mixture containing 12% cement achieved the highest volumetric expansion ratio and an average crack-width development rate of 2.35 mm/min. In summary, compared with conventional SCAs, adjusting the proportion of cementitious materials enables effective control over the hydration reaction rate and expansion performance of SCAs. This research provides valuable theoretical support for the design and application of high-performance SCA in rock and concrete demolition under complex engineering conditions.

1  Introduction

In recent decades, static cracking agent (SCA) has emerged as a greener and safer alternative to explosive blasting methods for demolitions of rock and concrete in engineering fields, owing to its advantages of low noise, minimal vibration, and absence of fly rock [1, 2].

...
References

1. Liu H, Li W, Guan W, Zhao H, Yao J, Wen Y. Mechanistic study of a microwave field-controlled static crushing agent for efficient rock breaking. ACS Omega. 2022;7(33):29344–55. doi:10.1021/acsomega.2c03598.

2. Al-Bakri A, Hefni M. A review of some nonexplosive alternative methods to conventional rock blasting. Open Geosci. 2021;13(1):431–42. doi:10.1515/geo-2020-0245.

3. Pal Roy P. Emerging trends in drilling and blasting technology: concerns and commitments. Arab J Geosci. 2021;14(7):652. doi:10.1007/s12517-021-06949-z.

4. Roy PP. Controlled blasting in mines & quarries—a paradigm. Curr Trends Civ Struct Eng. 2019;4(3):1–2. doi:10.33552/ctcse.2019.04.000589.

5. Laefer DF, Natanzi AS, Zolanvari SMI. Impact of thermal transfer on hydration heat of a soundless chemical demolition agent. Constr Build Mater. 2018;187(6):348–59. doi:10.1016/j.conbuildmat.2018.07.168.

6. Li S, Li Z, Luo M. Experimental study on reasonable composition and proportion of coal and rock static cracking agent. Blasting. 2018;35:137–53. (In Chinese). doi:10.3963/j.issn.1001-487X.2018.01.022.

7. Li C, He S, Hou W, Ma D. Experimental study on expansion and cracking properties of static cracking agents in different assembly states. Int J Min Sci Technol. 2022;32(6):1259–72. doi:10.1016/j.ijmst.2022.09.001.

8. Maneenoi N, Bissen R, Chawchai S. Influence of admixtures on the performance of soundless chemical demolition agents and implications for their utilization. J Sustain Min. 2022;21(2):93–111. doi:10.46873/2300-3960.1350.

9. Natanzi AS, Laefer DF, Connolly L. Cold and moderate ambient temperatures effects on expansive pressure development in soundless chemical demolition agents. Constr Build Mater. 2016;110(5):117–27. doi:10.1016/j.conbuildmat.2016.02.016.

10. Hua T, Cao Z, Zhang S, Guo R. Relationship between expansion and strength of cement paste with CaO-based expansive agent. Materials. 2024;17(24):6125. doi:10.3390/ma17246125.

11. Colombi P, D’Antino T. Analytical assessment of the stress-transfer mechanism in FRCM composites. Compos Struct. 2019;220(5):961–70. doi:10.1016/j.compstruct.2019.03.074.

12. Yang G, Wang H, Wan-Wendner R, Hu Z, Liu J. Cracking behavior of ultra-high strength mortar with CaO-based expansive agent and superabsorbent polymer. Constr Build Mater. 2022;357(6):129281. doi:10.1016/j.conbuildmat.2022.129281.

13. Li P, Nie GH. Study on the static cracking agent. J Hubei Univ Natl. 2012;2:159–62. (In Chinese).

14. AQ 1108-2014. Technical specification of static cracking for underground coal mine. Beijing, China: China Coal Industry Publishing House; 2014.

15. Li H, Liu JP, Tian Q, Zhang SZ. Hydration kinetics and microscopic analysis of calcium oxide expansion clinker. Appl Mech Mater. 2013;477–478:908–14. doi:10.4028/www.scientific.net/amm.477-478.908.

16. GB/T 8077-2023. Methods for testing uniformity of concrete admixtures. Beijing, China: Standards Press of China; 2023.

17. Zhang L, Ding D, Zhao J, Zhou G, Wang Z. Mixture design and mechanical properties of recycled mortar and fully recycled aggregate concrete incorporated with fly ash. Materials. 2022;15(22):8143. doi:10.3390/ma15228143.

18. Criado YA, Alonso M, Abanades JC. Kinetics of the CaO/Ca(OH)2 hydration/dehydration reaction for thermochemical energy storage applications. Ind Eng Chem Res. 2014;53(32):12594–601. doi:10.1021/ie404246p.

19. Tong C, Wang L, Wang K, Fu J. Early hydration kinetics of shell ash-based cementitious materials: a low-field nuclear magnetic resonance study. Materials. 2025;18(14):3253. doi:10.3390/ma18143253.

20. Seo JH, Park SM, Yang BJ, Jang JG. Calcined oyster shell powder as an expansive additive in cement mortar. Materials. 2019;12(8):1322. doi:10.3390/ma12081322.

21. Guo W, Zou S, Pu S, Zhou Y. Study on the physical and chemical properties of cement-based grout containing coal-fly ash. Materials. 2022;15(24):8804. doi:10.3390/ma15248804.

22. Hua T, Tang J, Zhu J, Tang H, Liu J. Evolution of the early compressive strength of cement-slag pastes with CaO-based expansive agent. Mater Struct. 2022;55(2):63. doi:10.1617/s11527-021-01809-4.

23. Cui F, Lei Z, Cheng X, Wu X, Shan P, Lv Z. Mechanism and application of static fracturing technology on deep working face. Adv Mater Sci Eng. 2021;2021(1):5516326. doi:10.1155/2021/5516326.

24. Alvarez JI, Veiga R, Martínez-Ramírez S, Secco M, Faria P, Maravelaki PN, et al. RILEM TC 277-LHS report: a review on the mechanisms of setting and hardening of lime-based binding systems. Mater Struct. 2021;54(2):63. doi:10.1617/s11527-021-01648-3.

25. Bogner A, Link J, Baum M, Mahlbacher M, Gil-Diaz T, Lützenkirchen J, et al. Early hydration and microstructure formation of Portland cement paste studied by oscillation rheology, isothermal calorimetry, 1H NMR relaxometry, conductance and SAXS. Cem Concr Res. 2020;130:105977. doi:10.1016/j.cemconres.2020.105977.

26. De Silva VRS, Ranjith PG, Perera MSA, Wu B, Rathnaweera TD. Investigation of the mechanical, microstructural and mineralogical morphology of soundless cracking demolition agents during the hydration process. Mater Charact. 2017;130:9–24. doi:10.1016/j.matchar.2017.05.004.

27. Gou J, Li S, Jiang C, Li Z, You G. A study on the influence of gypsum and Ca(OH)2 on the mechanical properties and hydration behavior of multi-component solid waste-based cementitious materials. Materials. 2025;18(9):1964. doi:10.3390/ma18091964.

28. Li H, Liu J, Wang Y, Tian Q. Simplified chemo-mechanical model of hydration/expansion of calcium-oxide-type expansive agent in cement-based materials. Mag Concr Res. 2020;72(19):1006–15. doi:10.1680/jmacr.18.00450.

29. Shen P, Lu L, He Y, Wang F, Lu J, Zheng H, et al. Investigation on expansion effect of the expansive agents in ultra-high performance concrete. Cem Concr Compos. 2020;105(6):103425. doi:10.1016/j.cemconcomp.2019.103425.

30. Huang L, Tang L, Löfgren I, Olsson N, Yang Z. Real-time monitoring the electrical properties of pastes to map the hydration induced microstructure change in cement-based materials. Cem Concr Compos. 2022;132:104639. doi:10.1016/j.cemconcomp.2022.104639.

31. Tas¸dog˘en AH, Dener M, Benli A, Balun B. Cold-cured alkali-activated slag/Portland cement composites: the role of cement content and alkali dosage on mechanical performance, microstructure, and sulfate durability. Struct Concr. 2026:70466. doi:10.1002/suco.70466.

32. Rahimi-Aghdam S, Masoero E, Rasoolinejad M, Bažant ZP. Century-long expansion of hydrating cement counteracting concrete shrinkage due to humidity drop from selfdesiccation or external drying. Mater Struct. 2019;52(1):11. doi:10.1617/s11527-018-1307-8.

33. Bentz DP, Stutzman PE. Curing, hydration, and microstructure of cement paste. ACI Mater J. 2006;103(5):348. doi:10.14359/18157.

34. Taylor HFW. Cement chemistry. 2nd ed. London, UK: Thomas Telford Publishing; 1997.

35. Tang S, Wang Y, Geng Z, Xu X, Yu W, Hubao A, et al. Structure, fractality, mechanics and durability of calcium silicate hydrates. Fractal Fract. 2021;5(2):47. doi:10.3390/fractalfract5020047.

36. Richardson IG. The nature of C-S-H in hardened cements. Cem Concr Res. 1999;29(8):1131–47. doi:10.1016/S0008-8846(99)00168-4.

37. Ioannidou K, Krakowiak KJ, Bauchy M, Hoover CG, Masoero E, Yip S, et al. Mesoscale texture of cement hydrates. Proc Natl Acad Sci U S A. 2016;113(8):2029–34. doi:10.1073/pnas.1520487113.

38. Wang J, Gao C, Tang J, Hu Z, Liu J. The multi-scale mechanical properties of calcium-silicate-hydrate. Cem Concr Compos. 2023;140:105097. doi:10.1016/j.cemconcomp.2023.105097.

Cite This Article

APA Style
Shao, J., Chen, P., Ma, Y., Wang, A., Tan, W. et al. (2026). Effect of cement content on the performance of static cracking agent. ZKG International, 79(7), 81–91. https://doi.org/10.32604/zkg.2026.077166
Vancouver Style
Shao J, Chen P, Ma Y, Wang A, Tan W, Tang D. Effect of cement content on the performance of static cracking agent. ZKG Int.. 2026;79(7):81–91. https://doi.org/10.32604/zkg.2026.077166
IEEE Style
J. Shao, P. Chen, Y. Ma, A. Wang, W. Tan, and D. Tang, “Effect of cement content on the performance of static cracking agent,” ZKG Int., vol. 79, no. 7, pp. 81–91, 2026. https://doi.org/10.32604/zkg.2026.077166

Related articles:

Issue 06/2025 US 2025/0187980 A1

Concrete having a low cement content

(22) 08.12.2022(43) 12.06.2025(57) The present invention relates to a fresh concrete compositioncomprising at least: i) a hydraulic binder comprising: from 20% to 40% by weight of Portland cement...

more
Issue 6/2022 WO 2022/123037 A1

Admixture for fluidifying a cementitious composition with reduced cement content

(22) 10.12.2021(43) 16.06.2022(57) The application describes an admixture containing a polymer as an agent for fluidifying a cementitious composition comprising: – from 20 to 64 wt% clinker; – from 5...

more
Issue 4/2018 US2018023268 (A1)

Test system and test method for detecting cement content of cement mixing pile body in real time

(22) 06.01.2016(43) 25.01.2018(57) The present invention discloses a test system and a test method for detecting the cement content of cement stirring pile body in real time at a construction site....

more
×