RU 2 730 820 C1

Method of extracting vanadium by countercurrent acid leaching of clinker from calcining firing

(22) 27.11.2019

(45) 26.08.2020

(57) Field: chemistry. Substance: invention relates to vanadium extraction technology, in particular to a method of extracting vanadium with countercurrent acid leaching of clinker, obtained as a result of calcining roasting. Method of extracting vanadium by countercurrent acid leaching of clinker, obtained as a result of calcining roasting, includes the stages: a. first leaching stage, on which clinker obtained as a result of calcining roasting is mixed, with a leaching liquid, adding sulphuric acid for the first leaching step, adjusting the pH value of the system at the first stage of the leaching process in range of 2.8 to 3.5, separation of solid phase from liquid to produce leach from first leaching stage and solid phase after leaching and washing solid phase to produce filtrate from first stage and solid substance; b. the second leaching stage, at which solid substance washed at stage a. is mixed with fluid for leaching at control of pH value of final system at the second leaching stage in range from 1.8 to 3.5 and separating solid phase from liquid phase to produce leachate from second leaching step and solid substance; c. third leaching stage, on which solid substance, leached and separated at stage b., mixed with a leaching liquid, which is represented by recycled water obtained after neutralization of waste water with lime or after electrolysis of waste water with a pH value of 0.7-1.5, when controlling the pH value of the final system at the third leaching stage in range of 1.4 to 2.2, separating the solid phase from the liquid phase to obtain leachate from the third leaching step and solid substance, and then washing the solid substance to obtain a filtrate from the third step and tailings after extraction of vanadium. Effect: method provides high rate of extraction of vanadium by leaching.

(73) Pangang Group Research Institute Co., Ltd. (CN)

x

Related articles:

Issue 2019-5 WO 2019/040995 A1

Mining method and mine

(22) 31.08.2018 (43) 07.03.2019 (57) A method of mining gypsum includes: in-situ leaching gypsum in a harvesting bed, such as a leach pad 5, in an existing gypsum resource with a leach liquor and...

more
Issue 2019-9 US 2019/0153347 A1

Method to reduce build-ups, crusts and ring formation in clinker production

(22) 29.06.2016 (43) 23.05.2019 (57) Some embodiments are directed to a method to avoid the negative effect of both sulphur and vanadium presence contained in solid fuel used in cement clinker...

more
Issue 2018-4 WO2018002690 (A1)

Method to reduce build-ups, crusts and ring formation in clinker production

(22) 29.06.2016 (43) 04.01.2018 (57) The present invention relates to a method to avoid the negative effect of both sulphur and vanadium presence contained in solid fuel used in cement clinker...

more
Issue 2016-12 US 2016/0304395 A1

Method for producing a pozzolanic or latent-hydraulic cement clinker substitute

(22) 04.12.2014 (43) 20.10.2016 (57) Methods for producing pozzolanic or latent hydraulic cement clinker substitutes may involve calcining clay with a fuel comprising a mineral substance at...

more
Issue 2017-5 WO 2017/045519 A1

Method for producing wet-process phosphoric acid and ­byproducing alpha-hemihydrate gypsum and high-purity and high-whiteness alpha-hemihydrate gypsum

(22) 26.08.2016 (43) 23.03.2017 (57) Provided is a method for producing wet-process phosphoric acid and by-producing alpha-hemihydrate gypsum and high-purity and high-whiteness alpha-hemihydrate...

more